美标H型钢W40*12*167
美标型钢:不得使用有损坏迹象的材料.材料进场后要核对规格与数量.检验管材是否有弯扁,劈裂现象,如有及时找厂家调换。搬运管材和管件时应小心轻放,避免油污,管材和管件应存放在通风良好的库房或简易棚内,不得露天存放,防止阳光直射,注意防火.管材应水平堆放在平整的地上,堆置高度不得过.5米。B.管道应铺设在经夯实的填土层内,填土层夯实后按管道埋设深度进行开挖,严禁在回填土之前或未经夯实的土层中铺设,铺设管道的沟底应平整。
美标H型钢尺寸表:
美标H型钢W12x4x14 A36/A992M/A572GR
美标H型钢W12x4x16 A36/A992M/A572GR
美标H型钢W12x4x19 A36/A992M/A572GR
美标H型钢W12x4x22 A36/A992M/A572GR
美标H型钢W12x6.5x26 A36/A992M/A572GR
美标H型钢W12x6.5x30 A36/A992M/A572GR
美标H型钢W12x6.5x35 A36/A992M/A572GR
美标H型钢W12x8x40 A36/A992M/A572GR
美标H型钢W12x8x45 A36/A992M/A572GR
美标H型钢W12x8x50 A36/A992M/A572GR
美标H型钢W12x10x53 A36/A992M/A572GR
美标H型钢W12x10x58 A36/A992M/A572GR
美标H型钢W12x12x65 A36/A992M/A572GR
美标H型钢W12x12x72 A36/A992M/A572GR
美标H型钢W12x12x79 A36/A992M/A572GR
美标H型钢W12x12x87 A36/A992M/A572GR
美标H型钢W12x12x96 A36/A992M/A572GR
美标H型钢W12x12x106 A36/A992M/A572GR
美标H型钢W12x12x120 A36/A992M/A572GR
美标H型钢W12x12x136 A36/A992M/A572GR
美标H型钢W12x12x152 A36/A992M/A572GR
美标H型钢型号表:
美标H型钢W12x12x170 A36/A992M/A572GR
美标H型钢W12x12x190 A36/A992M/A572GR
美标H型钢W12x12x210 A36/A992M/A572GR
美标H型钢W12x12x230 A36/A992M/A572GR
美标H型钢W14x5x22 A36/A992M/A572GR
美标H型钢W14x5x26 A36/A992M/A572GR
美标H型钢W14x6.75x30 A36/A992M/A572GR
美标H型钢W14x6.75x34 A36/A992M/A572GR
美标H型钢W14x6.75x38 A36/A992M/A572GR
美标H型钢W14x8x43 A36/A992M/A572GR
美标H型钢W14x8x48 A36/A992M/A572GR
美标H型钢W14x8x53 A36/A992M/A572GR
美标H型钢W16x7x57 A992、A36、A572
美标H型钢W16x10.25x67 A992、A36、A572
美标H型钢W16x10.25x77 A992、A36、A572
美标H型钢W16x10.25x89 A992、A36、A572
美标H型钢W16x10.25x100 A992、A36、A572
美标钢铁:为了增加咬入性,大型穿孔轧辊一般在入口锥上加工有深度为0.8~1.2mm的网状花纹。综合厂家的材质选择及使用情况,笔者认为:穿孔机轧辊选用铸造50Mn、60CrMnMo等中碳合金钢材质较合适,一是具有较好的强度及性,二是适用于轧制各种材质钢管。硬度控制在HB200-240较合理。3轧管机毛管轧制是热轧无缝钢管生产的主要变形工序,其作用是使毛管壁厚接近或达到成品管壁厚,和消除毛管在穿孔过程中产生的纵向壁厚不均,另外还可提高荒管内外表面质量,控制荒管外径和圆度。